The aim of this work is to study wearing of alloy 359.0 which are (Al-9%Si)
before and after heat treatment. First heat treatment is precipitation hardening
,Second Laser surface treatment ,The microstructure after precipitation process
and laser application effected on the hardness and wear rate.
|